Indium Corporation will feature its metal thermal interface materials for burn-in and test, including HSK patterned Heat-Spring®and HSMF-OS, at TestConX on March 3-6 in Mesa, Ariz.
A pure indium Heat-Spring®in the HSK pattern can be clad on one side with a thin layer of aluminum, which will prevent the indium from sticking to the device under test (DUT). Due to the thinness of the aluminum, it has minimal impact on the thermal conductivity of the indium.
HSMF-OS has a multi-layer construction with a total thickness of 0.004” that is designed for multiple insertions. It has an aluminum layer that acts as an interface with the DUT and has a tensile strength of approximately 90 MPa with a soft, compliant polymer backing. This unique construction results in a configuration with “designed-in” insertion survivability.
To learn more about Indium Corporation’s metal thermal interface materials for burn-in and test, visit indiumstg.wpenginepowered.com/BiTS.
Indium Corporation 是全球電子、半導體、薄膜和熱管理市場的主要材料製造商和供應商。產品包括焊料和助熔劑、銅钎、熱介面材料、濺鍍靶材、铟、鎵、錫金屬和無機化合物,以及 NanoFoil®。公司成立於 1934 年,擁有全球性的技術支援,工廠位於中國、馬來西亞、新加坡、南韓、英國和美國。
For more information about Indium Corporation, visit indiumstg.wpenginepowered.com or email [email protected]. You can also follow our experts, From One Engineer To Another®(#FOETA), at www.facebook.com/indium or @IndiumCorp.