Indium Corporation will feature its new high-performance, high-reliability alloy technology at PCB Carolina on November 13 in Raleigh, North Carolina, USA.
Durafuse™ LT is a novel, low-temperature alloy system designed to provide high-reliability in low applications that are looking for a reflow temperature below 210°C. Where traditional low-temperature solders often produce brittle solder joints that are susceptible to drop shock failures, Durafuse LT offers improved drop shock resilience, outclassing BiSn or BiSnAg alloys, and even performs better than SAC305 with optimum process setup. Durafuse LT:
- 為熱敏元件和柔性聚合物提供解決方案
- 防止處理器元件和多層板的熱彎曲
- Meets low temperature requirements for step soldering, particularly in RF shield attachment and rework applications
To learn more about Indium Corporation’s innovative low-temperature technology, stop by booth #76 or reach out to our Technical Support Engineers at [email protected].
Indium Corporation 是全球電子、半導體、薄膜和熱管理市場的主要材料製造商和供應商。產品包括焊錫和助熔劑、銅钎、熱介面材料、濺鍍靶材、铟、鎵、錫金屬和無機化合物以及 NanoFoil®。公司成立於 1934 年,擁有全球性的技術支援,工廠位於中國、印度、馬來西亞、新加坡、南韓、英國和美國。
如需進一步了解 Indium Corporation,請造訪indiumstg.wpenginepowered.com或發送電子郵件至 [email protected]。您也可以在www.facebook.com/indium或@IndiumCorp 追蹤我們的專家團隊「From One Engineer ToAnother®」(#FOETA)。