Indium Corporation, a leading materials refiner, smelter, manufacturer, and supplier to the global electronics, semiconductor, thin-film, and thermal management markets, will feature a range of innovative, high-reliability solder products for printed circuit board assembly (PCBA) at the SMTA Guadalajara Expo and Tech Forum, to be held September 17-18 in Guadalajara, Mexico.
铟泰公司 其推荐产品中展示以下产品:
- Durafuse® HR, a trusted and proven solder paste alloy technology, delivers enhanced thermal cycling capabilities (-40°C/125°C and -40°C/150°C) and superior voiding control for high-reliability automotive applications. It also offers reduced solder joint cracking and increased shear strength.
- Durafuse® LT is a solder paste alloy system with versatile characteristics that enable energy savings, high reliability, and low-temperature step soldering. It is ideal for assemblies with large temperature gradients and large BGAs with complex warpage profiles. Durafuse® LT delivers superior thermal cycling and drop shock performance, outperforming conventional low-temperature solders like BiSn or BiSnAg alloys, and can outperform SAC305 under optimal process conditions.
- Indium12.9HF is a no-clean, halogen-free solder paste specifically formulated to accommodate fine-feature printing, as seen with 01005 and 008004 components. It offers unprecedented stencil print transfer efficiency to work in the broadest range of processes to boost SPI yields. Indium12.9HF also delivers low voiding at BGA, CSP, LGA, and QFN, and high oxidation resistance without graping or solder balling on pads as small as 175 microns in air reflow.
- CW-807RS is a new high-reliability, halide- and halogen-free flux-cored wire that improves wetting speeds and cycle times for electronics assembly and robot soldering applications.
- CW-818 is a halide-free, no-clean cored wire with spatter control technology that provides fast wetting speeds to minimize cycle times in manual and robotic soldering processes.
To learn more about Indium Corporation’s high-reliability PCBA solder solutions, visit our experts at booth 901 during the SMTA Guadalajara Expo.
关于铟泰铟泰公司
铟泰公司®是面向全球电子、半导体、薄膜及热管理 顶级材料精炼商、冶炼商、制造商和供应商。产品包括焊料和助焊剂;硬钎焊;热界面材料;溅射靶材;铟、镓(Ga)、锗和锡金属及化合物;以及NanoFoil®。公司成立于1934年,拥有全球技术支持网络,并在中国、德国、印度、马来西亚、新加坡、韩国、英国和美国设有工厂。
For more information about Indium Corporation, visit indiumstg.wpenginepowered.com or email [email protected]. You can also follow our experts, From One Engineer To Another® (#FOETA), at www.linkedin.com/company/indium-corporation/.