Indium Corporation’s newly-patented BiAgX® solder paste technology is the only low-cost, lead-free replacement solder paste that is customer-proven to survive JEDEC/IPC J-STD-020  MSL1 preconditioning in specific devices without delamination.

BiAgX is a high-melting, lead-free (Pb-free) solder paste technology that serves as a drop-in replacement for the high-Pb solder pastes used in many high-reliability die-attach and electronics assembly applications.

BiAgX survives junction temperatures and high-temperature environments in excess of 175 °C, with minimal degradation of the mechanical structure and joint strength.

Environmental and legislative concerns are driving consumers away from products using solders that contain lead, including solders used in die-attach applications for analog semiconductor assembly. Customers have proven that BiAgX addresses these applications in a Pb-Free configuration.

“Our U.S. Patent has been approved. This and the other global patent applications ensure that BiAgX is the only low-cost solder solution for those ODM, OSAT, and other electronics assembly customers looking to replace high-lead containing solders,” said Indium Corporation’s Andy C. Mackie, PhD, MSc, Senior Product Manager for Semiconductor and Advanced Assembly Materials.

BiAgX is suited for small, low-voltage QFN packages that are used in portable electronics (smartphones/tablets), automotive electronics, and industrial applications. It requires minimal process adjustments and no capital expenditures for customers converting from a standard high Pb-containing solder paste-based process. It is both Pb-free and Sb-free (antimony-free) and does not contain costly specialty materials, such as nanosilver or sintering aids.

BiAgX reflows, solders, wets, and solidifies just like any other solder paste, and is available in both dispense and printing forms. Flux residues are easily cleanable with standard cleaning chemistries and processes.

For more information about BiAgX, including technical papers and other technical information, visit indiumstg.wpenginepowered.com/BiAgX.

铟泰公司 面向全球电子、半导体、太阳能、薄膜及热管理 顶级材料制造商和供应商。 产品包括焊料和助焊剂;硬钎焊;热界面材料;溅射靶材;铟、镓(Ga)、锗和锡的金属及化合物;以及NanoFoil®。铟泰公司成立于1934年,拥有全球技术支持体系,并在中国、马来西亚、新加坡、韩国、英国和美国设有工厂。

如需了解铟泰公司更多信息,请访问indiumstg.wpenginepowered.com或发送电子邮件至 [email protected]。您还可以通过www.facebook.com/indium或@IndiumCorp 关注我们的专家团队“From One Engineer ToAnother®”(#FOETA)。