Indium Corporation Launches New Water-Soluble, Halogen-Free Solder Paste

Indium Corporation has released Indium6.6HF Solder Paste – a new water-soluble solder paste that is compatible with both SnPb and Pb-free alloys. Indium6.6HF is designed to provide exceptional stencil printing performance and minimize voiding in PCB assembly applications. 

Indium6.6HF exhibits superior wetting to a variety of surface finishes resulting in the fewest voids, a reduction in the size of the largest voids, and minimized overall voiding. 

Other Indium6.6HF benefits include:

  • Halogen-free per IEC 61249-2-21 test method EN14582
  • Exceptional printing process window:
    • High transfer efficiency
    • Long stencil life (up to 12 hours)
    • Excellent response-to-pause
    • Prints consistently at a wide range of speeds
  • High tack value (>8 hours) ensures consistent component holding power, allowing high-speed component placement operation
  • Cleanable up to at least 72 hours after reflow

For more information about Indium6.6HF, visit: https://www.indium.com/solder-paste-and-powders/water-soluble-products/.  

铟泰公司 是一家面向全球电子、半导体、薄膜及热管理 市场的顶级材料制造商和供应商。产品包括焊料和助焊剂;硬钎焊 ;热界面材料;溅射靶材 ;铟、镓(Ga) 、锗和锡等金属及无机材料化合物 ;以及NanoFoil®。该公司成立于1934年,拥有全球技术支持网络,并在中国、马来西亚 、新加坡 、韩国、英国和美国设有工厂。