产品 合金 焊料合金

焊料合金

Since our founding in 1934, Indium Corporation has been a global leader in specialty solders and alloy development. Our research and development team, which includes many Ph.D. metallurgists, collaborates on our core metals to develop alloys that tackle current and emerging soldering and sealing challenges.

技术支持:铟泰公司

  • Patented Alloy Technologies
  • 世界一流的开发团队和实验室
  • 90 多年的经验
各种焊料合金

Application Expertise

Our global applications engineering teams are available for consultations to fully understand your unique needs.

各种形式

Most solder alloys can be supplied in the form of pastes, preforms, wires, bars, spheres, and more.

Mixed Alloy Technology

Our patented mixed alloy technology, Durafuse®, tackles the latest soldering challenges. Since its introduction, multiple products featuring this technology have evolved and been adopted by major OEMs, EMS providers, and OSATs.

Colorful arrows display temperature ranges for various soldering techniques using solder alloys 50 and 110, spanning from <30°C to >280°C.
Shiny, silvery liquid metal pooling and folding over a grey surface.

Liquid Metal for Thermal Interface (<30ºC)

  • Indalloy® 51E(GaInSn)
  • Indalloy® 60(GaIn)
  • Indalloy® 77(GaIn)
  • Indalloy® 300E(GaIn)
A white spiral-bound notebook with blue printed lettering lies on a dark surface.

Low-Temperature Solder and Sealing (30–210ºC)

  • Indalloy® 1E (InSn)
  • Indalloy® 4 (In)
  • Indalloy® 38(BiPbSn)
  • Indalloy® 117(BiPbInSnCd)
  • Indalloy® 227(SnInAg)
  • Indalloy® 254(SnInAg)
  • Indalloy® 281(BiSn)
  • Indalloy® 282(BiSnAg)
Silver-gray metal ingots, bars, and rods arranged on a surface.

传统焊接(150-260ºC)

  • Indalloy® 100(锡铅银)
  • Indalloy® 106(Sn63)
  • Indalloy® 121(锡银)
  • Indalloy® 241(SAC387)
  • Indalloy® 256(SAC305)
  • Indalloy® 276 (SnAg+)
  • Indalloy® 291 (SnCu+)
Gold bars stacked with glossy, reflective surfaces and warm lighting.

高温焊接(230-360ºC)

  • Indalloy® 133(SnSb)
  • Indalloy® 228(Sn10)
  • Indalloy® 266(HMP)
  • Indalloy® 292
Gold bars stacked with glossy, reflective surfaces and warm lighting.

Au and Braze Alloys (>280ºC)

  • Indalloy® 182(AuSn)
  • Indalloy® 183(金锗)
  • Indalloy® 193(银铜)
  • Indalloy® 200(金)

Six Solder Alloy Families

镓(Ga)

Indalloy®#组成Liquidus/Solidus Temperature (°C)
51EGa66.5/In20.5/Sn1311 共晶
300EGa78.6/In21.415.7 共晶

铋

Indalloy®#组成Liquidus/Solidus Temperature (°C)Solidus Temperature (°C)
281Bi58/Sn42138 共晶
282Bi57/Sn42/Ag1140139

铟

Indalloy®#组成Liquidus/Solidus Temperature (°C)Solidus Temperature (°C)
1EIn52/Sn48118 共晶
1In50/Sn50126118
290In97/Ag3143 共晶
2In80/Pb15/Ag5154149
4In100157 Melting Point
204In70/Pb30175165
205In60/Pb40181173
227Sn77.2/In20/Ag2.8187
7In50/Pb50210184
3In90/Ag10237143
164Pb92.5/In/Ag2.5310300

锡

Indalloy®#组成Liquidus/Solidus Temperature (°C)Solidus Temperature (°C)
106Sn63/Pb37 (Sn63)183 共晶
121Sn96.5/Ag3.5221 共晶
133Sn95/Sb5240237
256Sn96.5/Ag3/Cu0.5 (SAC305)220217

领导

Indalloy®#组成Liquidus/Solidus Temperature (°C)Solidus Temperature (°C)
151Pb92.5/Sn5/Ag2.5306298
164Pb92.5/In5/Ag2.5310300

Gold

Indalloy®#组成Liquidus/Solidus Temperature (°C)Solidus Temperature (°C)
182Au80/Sn20280 共晶
183Au88/Ge12356 共晶
184Au96.8/Si3.2363 共晶
200Au1001,064 Melting Point

焊料合金

Looking for a specific alloy? Visit our Solder Alloy Selector Guide to figure out which Indium Corporation alloy is right for your application, or download our Solder Alloy Directory to browse the available Indalloys.

相关应用

印刷电路板板上的微芯片

PCB

经过验证且处于行业前沿PCB 组装材料PCB

一辆未来感十足的白色跑车,搭载着先进的电力电子系统,在霓虹灯照亮的夜色中疾驰穿梭,展现着尖端的速度与科技。

电力电子产品包装与装配

种类齐全、经过验证的高可靠性 和……

高温焊接

高温焊接

为关键应用提供耐高温焊接材料应用

相关市场

焊料合金广泛应用于涉及电子组装或包装的行业。

您有技术问题或销售咨询吗?我们的专业团队随时为您提供帮助。From One Engineer to Another®不仅是我们的一句口号,更是我们致力于提供卓越服务的承诺。只要您需要,我们随时待命。让我们联系吧!

该图片的 alt 属性为空;文件名为 scientist-with-microscope.png

寻找安全数据表?

您所需的一切——从技术规格到应用 ——都可在此一站式获取。