铟泰公司的五位技术专家将于 2010 年 4 月 6 日至 9 日在内华达州拉斯维加斯举行的 APEX 展会上发表他们的技术研究成果。
- 李宁成,博士,技术副总裁
- 罗纳德·C·拉斯基,博士,注册工程师(PE),高级技术专家
- 马里奥·斯卡尔佐,高级技术支持工程师
- 埃里克·巴斯托,高级技术支持工程师
- 克里斯·安格林, 应用 开发工程师
李博士将发表三篇论文,其中包括《无铅助焊剂技术及其对清洗的影响》。无铅化、成本压力以及“多干净才算干净?”这一永无止境的问题,给装配作业带来了持续的挑战。本文将探讨这些挑战。
4月6日,星期二——下午1:30至3:00
叠层封装(PoP) 封装用浸渍助焊剂和焊膏的选择。本文探讨了市场前景、组装工艺方法以及为实现将新一代高性能分立逻辑器件和存储芯片 芯片 元件集成到单一封装外形中而发展起来的关键基础设施要素。
4月7日,星期三——上午10:15至11:45
通过锰(Mn)或铈(Ce)掺杂,实现高可靠性 、低成本无铅SAC焊点 。在本研究中,对掺有锰(Mn)或铈(Ce)的低银(Ag)SAC合金与共晶SnPb、SAC105和SAC305进行了对比评估,测试项目包括JEDEC跌落试验、动态弯曲试验、温度循环试验和循环弯曲试验。
4月7日,星期三——下午1:30至3:30
他还将主讲一门专业发展课程《实现高可靠性 的无铅焊点 ——材料考量》。本课程探讨了多种因素如何导致失效模式,以及如何选择合适的焊料合金和表面处理工艺,以实现高可靠性 。
4月9日,星期五——上午9:00——中午12:00
Dr. Lasky will be presenting a professional development course
Lead-Free Reliability
This course will cover how to develop a strategy for compliant electronic assembly with high yields and excellent reliability while complying with global environmental regulations.
· Thursday, April 8 – 9:00am – 12:00pm
Mario Scalzo; will be presenting the paper
Addressing the Challenge of Head-in-Pillow Defects in Electronics Assembly. This paper discusses the head-in-pillow failure mode and a strategy to minimize this troublesome defect.
· Wednesday, April 7 – 9:00 – 10:00am
He will also be presenting a paper authored by Tim Jensen
Challenges for Implementing a Halogen-Free Process.; Replacing halogenated compounds can have a dramatic affect on the PCB assembly process. This paper discusses those challenges, as well as techniques and practices that help ensure high end-of-line yields and continued reliability.
· Thursday, April 8 – 10:15 – 11:45am
Eric Bastow will be presenting
Understanding SIR. This paper will discuss the issue of SIR coupon preparation, board cleaning techniques, and how board cleanliness directly affects SIR results.
· Wednesday, April 7 – 10:15 – 11:45am
Chris Anglin will be presenting the paper
Stencil Printing Transfer Efficiency of Circular vs. Square Apertures with the Same Solder Paste Volume. This paper addresses the issues associated with stencil and squeegee design and the printing of paste for small passives.
· Thursday, April 8 – 10:15 – 11:45am
Indium Corporation is also exhibiting at booth #441.
Sponsored by IPC, this technical conference is known worldwide as one of the finest and most selective in the world.
Dr. Lee is a world-renown soldering expert and an SMTA Member of Distinction. He has extensive experience in the development of solder pastes, fluxes, high-temperature polymers, encapsulants for microelectronics, underfills, and adhesives. His current research interests cover advanced materials for interconnects and packaging for electronics and optoelectronics applications, with emphasis on both high-performance and low-cost of ownership. Dr. Lee is also a member of the SMTAI planning committee.
Dr. Lasky, holder of the prestigious SMTA Founder’s Award, is a world-renown process expert and an Instructional Professor at Dartmouth College. He has over 25 years of experience in electronics and optoelectronic packaging and assembly. He has authored or edited five books and numerous technical papers and holds several patent disclosures. Dr. Lasky also authors a technology blog which can be found at http://blogs.indium.com/blog/an-interview-with-the-professor.
Tim Jensen is the Product Manager for PCB Assembly Materials in Indium Corporation’s Solder Products Business Unit. He is an SMTA-Certified SMT Process Engineer. He has spent over a decade troubleshooting and optimizing SMT process lines. He works closely with Indium’s Technical Service, Research & Development, and Sales Teams to ensure that Indium continues to offer cutting edge products to meet unique challenges in the electronics assembly industry. Tim has a bachelor’s degree in Chemical Engineering from Clarkson University. He has authored several technical publications and numerous process and technical guidelines. Tim is a member of the SMTA and participates actively in several IPC standards development committees.
Eric Bastow joined Indium Corporation in 2001 developing new solder paste flux chemistries under the direction of Dr. Ning-Cheng Lee. He also gained experience performing residual gas analysis of hermetic electronic packages and developing electroless nickel-plating bath chemistries. Eric is an SMTA-certified process engineer (CSMTPE) and has earned his Six Sigma Green Belt from the Thayer School of Engineering at Dartmouth College. He has an associate’s degree in Engineering Science from the State University of New York and has authored several technical papers and articles.
Mario Scalzo joined Indium Corporation in 2000. He holds a bachelor’s degree in Chemistry from Saint Anselm College. He also holds a certificate from the American Chemical Society for Professional Education. In addition, he is an SMTA-Certified Process Engineer and has a Six-Sigma Black Belt from Dartmouth College’s Thayer School of Engineering. He is also the author of the Electronics Assembly Materials blog http://blogs.indium.com/blog/mario-scalzos-tech-support-blog.
Chris Anglin has over 15 years of experience in advanced process development, new product introduction, and electronics assembly manufacturing. He has a master’s degree in Industrial Engineering from the State University of New York at Binghamton. He is trained in Six Sigma Black Belt programs and is also an SMTA-Certified Process engineer.
For more information about the technical conferences and APEX, visit http://www.goipcshows.org.
Indium Corporation is a premiere materials supplier to the global electronics, semiconductor, solar, thin film and thermal management markets. Products include solders, preforms, and fluxes; brazes; sputter targets; indium, gallium, and germanium chemicals and sourcing; and Reactive NanoFoil®. Founded in 1934, Indium has global technical support and factories located in China, Singapore, South Korea, the United Kingdom, and the USA.
For more information about Indium Corporation, visit https://www.indium.com or email [email protected].