Indium Corporation will feature its ultra-reliable, void-reducing Indium8.9HF Solder Paste for automotive applications at SMTA International, September 22-26, Rosemont, Illinois, USA.
Indium8.9HF is a proven solder paste series that delivers no-clean, halogen-free solutions designed to produce low-voiding, enhanced electrical reliability, and improved stability during the printing process. It is specially formulated to accommodate the higher processing temperatures required by the SnAgCu, SnAg, and other alloy systems favored by the automotive electronics industry.Indium8.9HF:
- 在冷藏条件下,可在长达 12 个月的时间内保持稳定的印刷和回流焊性能
- 在室温下放置一个月后仍能保持出色的印刷和回流焊性能
- Delivers excellent response-to-pause printing performance even after being left on the stencil for 60 hours
- Performs with both Pb and Pb-free alloys
Indium8.9HF provides unique oxidation barrier technology that eliminates HIP defects and graping, making it perfectly suited for automotive applications. It is also able to enhance the reliability of automotive products in numerous ways:
- Exceeds all requirements for enhanced electrical reliability and SIR performance
- Improves thermal conductivity and thermal reliability with industry-proven low-voiding performance
- 防止助焊剂过早扩散,防止表面氧化
- Meets HKMC MS184-01 testing criteria Type B—one of the automotive industry’s most stringent reliability criteria
For information on Indium8.9HF and its use in the automotive industry, visit indiumstg.wpenginepowered.com/avoidthevoid or visit booth #515.
Indium Corporation is a premier materials manufacturer and supplier to the global electronics, semiconductor, thin-film, and thermal management markets. Products include solders and fluxes; brazes; thermal interface materials; sputtering targets; indium, gallium, germanium, and tin metals and inorganic compounds; and NanoFoil®. Founded in 1934, the company has global technical support and factories located in China, Malaysia, Singapore, South Korea, the United Kingdom, and the USA.
如需了解铟泰公司更多信息,请访问indiumstg.wpenginepowered.com或发送电子邮件至 [email protected]。您还可以通过www.facebook.com/indium或@IndiumCorp 关注我们的专家团队“From One Engineer ToAnother®”(#FOETA)。