焊接 TIM (sTIM)

High-power density devices demand top-tier thermal interface materials. Indium Corporation’s sTIMs meet the reliability, thermal, and warpage requirements of high-performance devices. As the leading global provider of sTIM solutions, we offer expertise in integrating sTIMs into your process, backed by our skilled engineers and trusted equipment partners.

技术支持:铟泰公司

  • 高度自动化的全球生产基地与稳定的长期供应链
  • Advanced Quality Controls Essential for Meeting Semiconductor Industry Standards
  • Global Network of Expert Technical Support
This illustration shows an exploded view of a chip package with a metal lid lifted above a green.

高热导率

Indium has a high bulk thermal conductivity (86 W/mK), which means less sensitivity to bondline thicknesses and coplanarity issues compared to polymer-based TIMs.

TIM1 和 TIM1.5 sTIM 解决方案

Indium and indium-based alloys are available for single and multiple reflow processes, designed for maximum wetting to various metallizations with minimal voiding.

长期可靠性

We’ll help you design and adopt a package architecture that ensures thermal and mechanical reliability to overcome both overheating and warpage.

High-Performance

Our sTIMs deliver the lowest total thermal resistance in the industry.

Manufactured Globally

Our manufacturing capabilities ensure high-quality product availability at scale across the globe.

可持续发展

We source our materials reliably and responsibly and offer reclaim and recycle programs. 

产品数据表

铟基焊料热界面材料 PDS 100407 R0
用于 BGA 封装的焊接热界面材料 PDS 100082 R1.pdf

相关应用

一张带有透明覆盖层的微芯片插图,展示了内部元器件 电子连接,突显了其堪比腕表设计的精密程度。

计时器 1、计时器 1.5、计时器 2

金属基热界面材料(TIM)具有出色的导热性能,并且……

一张电路板 上的计算机微芯片特写电路板 可见电子元器件 电路图案。

热管理

面向高性能计算(HPC)的散热解决方案,确保可靠性

Exploded view of electronic components on a green background, showing circuit boards, copper connectors, and a central logo.

包装-附件

广泛的选择以应对……的挑战

相关市场

您有技术问题或销售咨询吗?我们的专业团队随时为您提供帮助。From One Engineer to Another®不仅是我们的一句口号,更是我们致力于提供卓越服务的承诺。只要您需要,我们随时待命。让我们联系吧!

该图片的 alt 属性为空;文件名为 scientist-with-microscope.png

寻找安全数据表?

您所需的一切——从技术规格到应用 ——都可在此一站式获取。