Indium Corporation® will feature its high-reliability, Au-based precision die-attach preforms for critical laser and RF applications at SPIE Photonics West, Jan. 28-30, in San Francisco, California. SPIE West is the world’s premier event for lasers, biomedical optics, biophotonic technologies, quantum, and optoelectronics.
Indium Corporation will showcase the following products:
- AuLTRA® Precision Die-Attach Preforms offer the NEW Gold Standard – the highest level of quality available to deliver the best performance possible in critical, high-reliability die-attach applications. Features include:
- Highly accurate thickness control
- Precise edge quality
- Optimized cleanliness
- Default waffle pack method
- Available for gold-based alloys
- AuLTRA® 75 is an off-eutectic AuSn preform solution (75Au/25Sn) designed to improve intermetallic reliability in applications using a die with a thicker gold plating, such as a GaN die used for high-frequency, high-power RF power amplifier devices for 5G and other critical military and aerospace wireless communications. AuLTRA® 75 helps improve the operation of these critical technologies by adjusting the final solder joint composition and improving wetting and voiding. The AuLTRA® 75 product line also comes in 78Au/22Sn and 79Au/21Sn compositions.
- AuLTRA® ThInFORMS are 0.00035″-thick (0.00889mm or 8.89μm) 80Au/20Sn preforms that improve the overall operational efficiency of high-output lasers. AuLTRA® ThInFORMS help combat common issues such as shorting and poor thermal transfer.
- AuLTRA® Fine Ribbon is the company’s Indalloy®182 fine-grade precision ribbon for high-volume, fully automated laser diode assembly processes. For these auto-feed systems, the precision and high quality of the ribbon and spooling are of the utmost importance along with long, continuous lengths. These features help minimize production downtime and facilitate an efficient, high-throughput process resulting in a high-quality end product and low cost of ownership.
- AuLTRA® 3.2 is an air or nitrogen reflow, water-soluble AuSn solder paste, optimized to handle the elevated processing temperatures of gold-based alloys. Perfect for high-power LED module array assemblies, it ensures consistent and repeatable printing performance, featuring a long stencil life and excellent tack. Along with consistently meeting printing and reflow demands, AuLTRA® 3.2 delivers superb wetting and low voiding.
- AuLTRA®5.1 is a no-clean AuSn solder paste, specifically formulated to endure the higher temperatures required by Au-based alloys. Ideal for high-power LED module array assemblies, this formulation provides a broad processing window and consistent print definition, even for ultra-fine pitches. Additionally, AuLTRA® 5.1 excels in wetting performance and void minimization, while meeting rigorous printing and reflow standards.
- Heat-Spring® is a compressible, non-reflow metal TIM ideal for TIM2 applications. These indium-containing TIMs offer superior thermal conductivity over non-metals, with pure indium metal delivering 86W/mK in all planes. Because of its sold metal state, Heat-Spring® avoids pump-out and bake-out problems. It also offers a sustainable solution due to the company’s indium reclaim and recycle program.
To learn more about Indium Corporation’s precision Au-based preforms, visit indiumstg.wpenginepowered.com/products/gold-solder/gold-alloy-preforms or stop by booth #4923 at the show.
About Indium Corporation
Indium Corporation® is a premier materials refiner, smelter, manufacturer, and supplier to the global electronics, semiconductor, thin-film, and thermal management markets. Products include solders and fluxes; brazes; thermal interface materials; sputtering targets; indium, gallium, germanium, and tin metals and inorganic compounds; and NanoFoil®. Founded in 1934, the company has global technical support and factories located in China, Germany, India, Malaysia, Singapore, South Korea, the United Kingdom, and the U.S.
For more information about Indium Corporation, visit indiumstg.wpenginepowered.com or email [email protected]. You can also follow our experts, From One Engineer To Another® (#FOETA), at www.linkedin.com/company/indium-corporation/.